Anybody seen this technique used? From the EAA experimenter.
" George ........... and he offered me a bit of a tip that I havenât come across
yetâmixing graphite with epoxy to provide a long-lasting smooth bearing
surface for the control torque tube. Hemixed a spreadable batch and
applied it to both surfaces and then pressed them lightly together with
wax paper between as a parting agent. "
" George ........... and he offered me a bit of a tip that I havenât come across
yetâmixing graphite with epoxy to provide a long-lasting smooth bearing
surface for the control torque tube. Hemixed a spreadable batch and
applied it to both surfaces and then pressed them lightly together with
wax paper between as a parting agent. "